PSAS/ ParaffinSpinCasting

Spin Casting

We will attempt to pour the liquid paraffin in a sealed cylindrical mold and spin this between 1000-3000 rpm until the paraffin has solidified and the shrinkage has created the right diameter port in the center of the grain.

The new technique uses the lathe to spin the grain, while molten paraffin is introduced through a hole at one end of the spinning assembly. The end cracking and surface cracking issues we have seen in the past are now resolved. (2005.7)


Tests
firstspincasting.pdf Results from first test
secondspincasting.pdf Results from second test
thirdspincasting.pdf Results from third test
forthspincasting.pdf Results from fourth test